some not-so-important alloys i made that aren't really special enough to get a name or their own save
layered strong crmc alloy material kyalloys stacking stacked layering tough

Comments

  • abh
    abh
    20th Jan 2021
    I think the durability is (L2R) 1>3>4>2
  • KyYay
    KyYay
    19th Jan 2021
    well when i test bombs on them the leftmost one is usually the one that survives
  • TotallyNotACat_
    TotallyNotACat_
    19th Jan 2021
    mid right is the only alloy to break bc of pressure
  • TotallyNotACat_
    TotallyNotACat_
    19th Jan 2021
    and left is second strongest
  • TotallyNotACat_
    TotallyNotACat_
    19th Jan 2021
    midleft is weakest right is strongest
  • KyYay
    KyYay
    19th Jan 2021
    imo the one on the left is the best, it cools very quickly
  • Anty
    Anty
    19th Jan 2021
    I noticed that Icum is probably the weakest and sparkium acctually might be stronger than crisscrossium as far as DEST goes
  • plutoniumfusion
    plutoniumfusion
    19th Jan 2021
    Everything!
  • Anty
    Anty
    18th Jan 2021
    which one plut
  • plutoniumfusion
    plutoniumfusion
    18th Jan 2021
    Wow. Finally an alloy that wind my bombs without cheater converter :O